Difference between revisions of "Serenity/Metal Treatment"
From A Wiki in the Desert
(One intermediate revision by the same user not shown) | |||
Line 11: | Line 11: | ||
*'''Steel : Stainless, Purity 7''': 20 Potash, 30 Saltpeter | *'''Steel : Stainless, Purity 7''': 20 Potash, 30 Saltpeter | ||
*'''Iron : Hard, corrosion Resistant''': 110 Saltpeter, 10 Cactus Sap | *'''Iron : Hard, corrosion Resistant''': 110 Saltpeter, 10 Cactus Sap | ||
+ | *'''Sun Steel : Hard, Stainless, Insulative''': 130 Saltpeter, 30 Gravel | ||
+ | *'''Cobalt : Hard, Stainless''': 90 Saltpeter | ||
(1) Only needed for the first gold plating treatment, to add gold metal salts to the acid. | (1) Only needed for the first gold plating treatment, to add gold metal salts to the acid. |
Latest revision as of 04:36, 18 February 2024
Back to Serenity
Metal Treatment Recipes for Tank 1 (don't use any other metal salts than gold for this tank)
k-values: 4.187 - 4.891 - 4.062 - 4.854 - 4.782 - 4.782 - 4.704 - 4.141
- Sun Steel : Insulated, Stainless: 20 Potash, 50 Gravel
- Sun Steel : Insulated, Corrosion Resistant: 20 Potash, 20 Gravel
- Moon Steel : Hard, Stainless, Purity 6: 10 Lime 50 Potash 50 Saltpeter
- Nickel : Gold Plated, Insulated, Stainless, Non-toxic, Purity 10: 60 Salt, 40 Potash, 70 Gravel, 10 Salts of Gold(1), 30 Coal, 10 Cabbage Juice, 20 Lime, 10 Gravel
- Steel : Stainless, Purity 7: 20 Potash, 30 Saltpeter
- Iron : Hard, corrosion Resistant: 110 Saltpeter, 10 Cactus Sap
- Sun Steel : Hard, Stainless, Insulative: 130 Saltpeter, 30 Gravel
- Cobalt : Hard, Stainless: 90 Saltpeter
(1) Only needed for the first gold plating treatment, to add gold metal salts to the acid.