Metal Treatment Recipes for Tank 1 (don't use any other metal salts than gold for this tank)
k-values: 4.187 - 4.891 - 4.062 - 4.854 - 4.782 - 4.782 - 4.704 - 4.141
- Sun Steel : Insulated, Stainless: 20 Potash, 50 Gravel
- Sun Steel : Insulated, Corrosion Resistant: 20 Potash, 20 Gravel
- Moon Steel : Hard, Stainless, Purity 6: 10 Lime 50 Potash 50 Saltpeter
- Nickel : Gold Plated, Insulated, Stainless, Non-toxic, Purity 10: 60 Salt, 40 Potash, 70 Gravel, 10 Salts of Gold(1), 30 Coal, 10 Cabbage Juice, 20 Lime, 10 Gravel
(1) Only needed for the first gold plating treatment, to add gold metal salts to the acid.