Difference between revisions of "Compression Furnace"
From A Wiki in the Desert
m (Added new, more obvious template indicating T7 content) |
m (clean up) |
||
Line 3: | Line 3: | ||
{{T7 Warning}} | {{T7 Warning}} | ||
− | {{ | + | {{BuildingInfo|image=CompressionFurnace.png|size=15x11|where=[[Compound]]|description=Used for making metals from ore.}} |
− | == | + | == Sources == |
This building becomes available after you have learned the [[Metallurgy]] tech. | This building becomes available after you have learned the [[Metallurgy]] tech. | ||
− | Compare all [[Furnace | + | Compare all [[Furnace]]s. |
Line 32: | Line 32: | ||
*Holds up to 20 [[Charcoal]] | *Holds up to 20 [[Charcoal]] | ||
*Burns 1 [[Charcoal]] per minute for a maximum of 20 minutes | *Burns 1 [[Charcoal]] per minute for a maximum of 20 minutes | ||
− | *The theoretical time to generate one metal appears to be 40000 / ore amount. The actual time is modified by rounding. (See the [[Talk: | + | *The theoretical time to generate one metal appears to be 40000 / ore amount. The actual time is modified by rounding. (See the [[Talk:Compression Furnace|discussion]] page for more details.) |
Revision as of 01:41, 26 July 2018
Sources
This building becomes available after you have learned the Metallurgy tech.
Compare all Furnaces.
Cost
- 100 Clay
- 3 Crucible
- 200 Firebricks
- 5 Iron Bars
Use
- Smelt any ore to produce metal. For example:
- Smelt Copper Ore to produce Copper
- Smelt Iron Ore to produce Iron
- Smelt Tin Ore to produce Tin
- Smelt Lead Ore to produce Lead
Uses Charcoal for fuel.
Operation
- Holds up to 500 ore
- Holds up to 20 Charcoal
- Burns 1 Charcoal per minute for a maximum of 20 minutes
- The theoretical time to generate one metal appears to be 40000 / ore amount. The actual time is modified by rounding. (See the discussion page for more details.)
Recipes
Confirmed | Ore | Charcoal | Metal Result | % Yield (Metal per Ore) | CC per Metal | Clinker |
---|---|---|---|---|---|---|
Yes | 500 | 20 | 15 | 3.0 | 1.33 | |
Yes | 500 | 19 | 15 | 3.0 | 1.27 | |
Yes | 500 | 16 | 12 | 2.4 | 1.33 | 488 |
Yes | 500 | 15 | 12 | 2.4 | 1.25 | |
Yes | 500 | 14 | 11 | 2.2 | 1.27 | |
Yes | 500 | 13 | 10 | 2.0 | 1.3 | |
Yes | 500 | 10 | 8 | 1.6 | 1.25 | |
Yes | 500 | 4 | 3 | 0.6 | 1.333 | |
Yes | 500 | 3 | 3 | 0.6 | 1 | |
Yes | 500 | 2 | 2 | 0.4 | 1 | |
Yes | 500 | 1 | 1 | 0.2 | 1 | |
Yes | 484 | 20 | 15 | 3.1 | 1.33 | |
Yes | 483 | 20 | 14 | 2.9 | 1.43 | |
Yes | 483 | 19 | 14 | 2.9 | 1.36 | |
Yes | 466 | 20 | 14 | |||
Yes | 390 | 20 | 12 | 3.08 | 1.67 | |
Yes | 300 | 13 | 6 | 2.0 | 2.17 | |
200 | 20 | 6 | 3.0 | 3.33 | ||
200 | 19 | 6 | 3.0 | 3.17 |
Note: the 200 ore/18 charcoal was performed by opening the furnace at about 18:15 into the process recovering left over charcoal and metal.
|