Difference between revisions of "Compression Furnace"
From A Wiki in the Desert
m (Removing old Languages template) |
m (→top: smwifying) |
||
Line 6: | Line 6: | ||
| name = Compression Furnace | | name = Compression Furnace | ||
| image = CompressionFurnace.png | | image = CompressionFurnace.png | ||
− | | location = [[Compound]] | + | | location = [[requires::Compound]] |
| size = 15 × 11 | | size = 15 × 11 | ||
| requirements = | | requirements = | ||
− | * [[Metallurgy]] | + | * [[requires::Metallurgy]] |
− | | material1 = [[Clay]] | + | | material1 = [[requires::Clay]] |
| qty1 = 100 | | qty1 = 100 | ||
− | | material2 = [[Crucible]] | + | | material2 = [[requires::Crucible]] |
| qty2 = 3 | | qty2 = 3 | ||
− | | material3 = [[Firebricks]] | + | | material3 = [[requires::Firebricks]] |
| qty3 = 200 | | qty3 = 200 | ||
− | | material4 = [[Iron Bars]] | + | | material4 = [[requires::Iron Bars]] |
| qty4 = 5 | | qty4 = 5 | ||
}} | }} |
Revision as of 15:19, 19 September 2019
Compression Furnace | ||||||||||
---|---|---|---|---|---|---|---|---|---|---|
(Building) | ||||||||||
Location | ||||||||||
Compound | ||||||||||
Size | ||||||||||
15 × 11 | ||||||||||
Requirements | ||||||||||
|
Sources
This building becomes available after you have learned the Metallurgy tech.
Compare all Furnaces.
Cost
- 100 Clay
- 3 Crucible
- 200 Firebricks
- 5 Iron Bars
Use
- Smelt any ore to produce metal. For example:
- Smelt Copper Ore to produce Copper
- Smelt Iron Ore to produce Iron
- Smelt Tin Ore to produce Tin
- Smelt Lead Ore to produce Lead
Uses Charcoal for fuel.
Operation
- Holds up to 500 ore
- Holds up to 20 Charcoal
- Burns 1 Charcoal per minute for a maximum of 20 minutes
- The theoretical time to generate one metal appears to be 40000 / ore amount. The actual time is modified by rounding. (See the discussion page for more details.)
Recipes
Confirmed | Ore | Charcoal | Metal Result | % Yield (Metal per Ore) | CC per Metal | Clinker |
---|---|---|---|---|---|---|
Yes | 500 | 20 | 15 | 3.0 | 1.33 | |
Yes | 500 | 19 | 15 | 3.0 | 1.27 | |
Yes | 500 | 16 | 12 | 2.4 | 1.33 | 488 |
Yes | 500 | 15 | 12 | 2.4 | 1.25 | |
Yes | 500 | 14 | 11 | 2.2 | 1.27 | |
Yes | 500 | 13 | 10 | 2.0 | 1.3 | |
Yes | 500 | 10 | 8 | 1.6 | 1.25 | |
Yes | 500 | 4 | 3 | 0.6 | 1.333 | |
Yes | 500 | 3 | 3 | 0.6 | 1 | |
Yes | 500 | 2 | 2 | 0.4 | 1 | |
Yes | 500 | 1 | 1 | 0.2 | 1 | |
Yes | 484 | 20 | 15 | 3.1 | 1.33 | |
Yes | 483 | 20 | 14 | 2.9 | 1.43 | |
Yes | 483 | 19 | 14 | 2.9 | 1.36 | |
Yes | 466 | 20 | 14 | |||
Yes | 461 | 20 | 14 | |||
Yes | 460 | 20 | 14 | |||
Yes | 459 | 20 | 14 | |||
Yes | 458 | 20 | 14 | |||
Yes | 400 | 20 | 12 | |||
Yes | 399 | 20 | 12 | 1.67 | ||
Yes | 390 | 20 | 12 | 3.08 | 1.67 | |
Yes | 358 | 20 | 11 | |||
Yes | 344 | 20 | 10 | |||
Yes | 300 | 13 | 6 | 2.0 | 2.17 | |
200 | 20 | 6 | 3.0 | 3.33 | ||
200 | 19 | 6 | 3.0 | 3.17 |
Note: the 200 ore/18 charcoal was performed by opening the furnace at about 18:15 into the process recovering left over charcoal and metal.
|